From: Low temperature vaporized hydrogen peroxide sterilization of 3D printed devices
Test Name | Sterilization Method / % Change | This study | |
---|---|---|---|
121 °C Steam. 20 min % change | 134 °C Steam, 10 min % change | ||
Tensile Strength | -4% | 15% | -1.8% (V) -14.7% (H) |
Flexural Strength | 0 to -7% | -44 to 14 | -17.2% (V) -14.4% (H) |
Hardness | -2% | 12% | 1.2% |